I. Flow control layer: PET molecular-level homogeneous filling
1. Multi-stage shear control hot runner
The conical tapered torpedo head is used to reduce the melt shear rate gradient by 80% and eliminate flow lines.
Measured: The maximum weight difference of 48-hole preforms in the same mold cavity is ≤0.03g (traditional molds>0.15g).
2. Nano-level surface tension balance
The surface of the mold cavity is treated with micro-nano composite texture (Ra=0.05μm)
II. Thermal balance layer: ±0.5℃ temperature control revolution
| Technical module | Implementation principle | Precision improvement effect |
| Dynamic variable diameter water channel | Differentiate the design of water channel diameter based on the mold cavity thermal map | Mold cavity temperature difference from ±8℃→±0.5℃ |
| Titanium alloy heat diffuser | Embed high thermal conductivity titanium sheet (λ=120W/mK) | Bottle bottom cooling efficiency increased by 40% |
| AI temperature control compensation | Real-time monitoring → automatic adjustment of cooling flow | Crystallinity fluctuation ≤3% (industry average 15%) |
Empirical data: The standard deviation of the inner diameter of the preform mouth is compressed from ±10μm to ±1.5μm (meeting the airtightness requirements of carbonated beverage bottle caps).
III. Digital compensation layer: "prophetic system" for predicting deformation
1. Dynamic prediction engine for shrinkage rate
Input material grade (PET/rPET/PP) → Automatically load 3000+ sets of historical shrinkage rate curves → Generate compensation coefficient.
Example: The shrinkage rate compensation value of rPET material is 0.18% higher than that of traditional molds.
2. Deformation reverse compensation processing
Preset deformation compensation amount (resolution 1μm) during CNC processing
Ensure that the mold cavity size still meets the tolerance when the mold is working at 155℃.